Abstract

This paper discusses applications of spherical nanoindentation stress-strain curves in characterizing the local mechanical behavior of materials with modified surfaces. Using ion-irradiated tungsten as a specific example, this paper demonstrates that a simple variation of the indenter size (radius) can identify the depth of the radiation-induced-damage zone, as well as quantify the behavior of the damaged zone itself. Using corresponding local structure information from electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM) we look at (a) the elastic response, elasto-plastic transition, and onset of plasticity in ion-irradiated tungsten, zirconium and 304 stainless steel under indentation, and compare their relative mechanical behavior to the unirradiated state, (b) correlating these changes to the different grain orientations as a function of (c) irradiation from different sources (such as He, W, and He+W for tungsten samples).

Original languageEnglish (US)
Title of host publicationProceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems – Water Reactors
EditorsDenise Paraventi, Michael Wright, John H. Jackson
PublisherSpringer International Publishing
Pages617-635
Number of pages19
ISBN (Print)9783319672434
DOIs
StatePublished - 2018
Event18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors, 2017 - Portland, United States
Duration: Aug 13 2017Aug 17 2017

Publication series

NameMinerals, Metals and Materials Series
VolumePart F9
ISSN (Print)2367-1181
ISSN (Electronic)2367-1696

Other

Other18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors, 2017
Country/TerritoryUnited States
CityPortland
Period8/13/178/17/17

Bibliographical note

Publisher Copyright:
© The Minerals, Metals & Materials Society 2018.

Keywords

  • Electron back-scattered diffraction
  • Nanoindentation stress-strain
  • Radiation damage gradient
  • Stress saturation
  • Transmission electron microscopy

Fingerprint

Dive into the research topics of 'Spherical nanoindentation stress-strain analysis of ion-irradiated tungsten'. Together they form a unique fingerprint.

Cite this